Re-varnishing the saloon table on an Oceanranger by Ian Buchanan

The Covid shutdown meant that extra time was available for home and boat projects – provided you did not need to go to the boat!

So, before the impending movement restrictions came into force, I removed the saloon table from my boat and took it home to re-varnish it.

My boat is a 1991 Oceanranger, with the mast stepped through the saloon table.

The first tip is to gently cut the old varnish where the capping for the mast rests on the centre of the table. This is to prevent (reduce in my case) the danger of lifting the veneer from the tabletop.

The two wings of the table were removed before the centre section was dismantled. It breaks down into two main parts, which can be further dismantled for the varnishing work.

Normally with varnish I use extra strength Nitromors, removing the ‘gunge’ by scraper then medium steel wool.

However, the varnish on my boat did not dissolve with Nitromors.

Having learned from previous experience of re-varnishing the cockpit table, the old varnish should not be removed by sanding as the veneer is ‘paper thin’ and easily rubbed through.

So it meant using a hot-air gun to soften and remove the varnish.  If you have not used this technique before, it takes some practice.  My own experience of such a technique started in the days of blowtorches – a much riskier pursuit!!!!

The modern hot-air guns have a temperature control, so there is less risk of burning the wood.  But it still takes care and practice.  The scraper used to remove the soft varnish needs to be ‘sharp’.  By this I mean not sharp like a chisel, but squared off cleanly/sharply (like a well dressed screwdriver) so that it cuts off the old varnish in a continuous strip, working along as the old varnish starts to bubble.

Having removed the old varnish by this method the wood is left relatively clean.  It can then be lightly sanded (working with the grain of the wood) before cleaning down with white spirit.

Once satisfied with the clean (and dry) wood it can be ‘primed’ with a light coat of varnish reduced with 50:50 thinners.

Matching the semi-gloss of the Westerly varnish is not easy.  I ended up using a 50:50 mix of International Original varnish and International Satin varnish, which suited me, although it was still glossier than before.  5 or 6 coats of varnish did the trick, and the end result satisfactory. Figure 1 – The finished table

[envira-gallery id="188193"]

and in other news…

60th Annual General Meeting

60th Annual General Meeting

The WOA’s 60th Annual General Meeting takes place in February 2027. Sign in to view the full details on the event page.

Chainplates

Chainplates

A Westerly Corsair was dismasted outside Brighton in July 2025 after its aft lower chainplate failed. Inspection found stress-corrosion cracking in a U-bolt that had been holding the chainplate by only a tiny fraction.

WOA 60th Anniversary Celebrations

WOA 60th Anniversary Celebrations

The South Coast Group kicked off this year’s celebrations with a rally that started in Yarmouth on the Isle of Wight on 15th June and finished in Portsmouth a week later. Twenty-four Westerlys assembled in Yarmouth during the day. The first pontoon party of the rally...